Research Article
Mechanical Properties of Lightweight Concrete Partition with a Core of Textile Waste
Table 3
The values of first-crack strength, first-crack deflection, toughness indices, and residual strength factors of bending specimens.
| Specimen code | Age at test |
First-crack strength (kgf) |
First-crack deflection | Toughness indices | Residual strength factor | | | | | |
| PC2 | 28 days | 563.7 | 0.335 | — | — | — | — | — | FPC25 | 28 days | 459 | 0.333 | 4.23 | 6.84 | 9.20 | 52.2 | 23.6 | FPC26 | 28 days | 373 | 0.313 | 3.94 | 5.94 | 8.97 | 40 | 30.3 |
|
|