Case Study of Remaining Service Life Assessment of a Cooling Water Intake Concrete Structure in Indonesia
Table 5
Corrosion thickness of rebar.
| Number | Code | Rebar diameter | Train | Corrosion thickness | Corrosion rate (mm/year) | Microstructure |
| 1 | Core 3 | 19 | A/B | 10~20 µm | 0.0003–0.0006 | Pearlite and Ferrite | 2 | Core 8 | 19 | C/D | 20~50 µm | 0.0007–0.0017 | Pearlite and Ferrite | 3 | Core 15 | 19 | G/H | 3~8 mm | 0.1875–0.5 | Pearlite and Ferrite |
|
|