Research Article
Assessing Mechanical Properties of Hot Mix Asphalt with Wire Wool Fibers
Table 1
Physical properties of the used asphalt cement.
| Property | Value |
AASHTO specifications for 60/70 penetration asphalt | Minimum | Maximum |
| Penetration (0.1 mm) | 66 | 60 | 70 | Flash point (°C) | 320 | 232 | — | Ductility at 25°C (cm) | 134 | 100 | — | Specific gravity at 25°C | 1.032 | 1.01 | 1.06 | Softening point (°C) | 53 | 48 | 56 | Penetration of residue (% of original) | 66 | 54 | — | Weight loss on heating (%) | 0.58 | | 0.8 |
|
|