Research Article

Behavior of Low Grade Steel Fiber Reinforced Concrete Made with Fresh and Recycled Brick Aggregates

Figure 15

Normalized stress-strain diagram at 7 day; (a) 0.5% SF and (b) 1% SF.
(a)
(b)