Review Article

Structural Glass Systems under Fire: Overview of Design Issues, Experimental Research, and Developments

Figure 9

Glass enclosures under fire. (a) Evidence of partial delamination, as reported in [60] and (b) full-scale glazing wall tested in [70]. In evidence, it is possible to notice the loss of wall integrity and initiation of gel melting, after 49 minutes of fire exposure.