Research Article
Efficient Adaptive Test Method for Textile Development Length in TRC
Table 1
Parameter specification of 1st batch of specimen.
| Textile | Material | Yarn fineness1 | Yarn distance1 | Weave, loop length2 | Coating type | Percentage of coating3 | (tex) | (mm) | (mm) |
| A | AR glass | 1280/640 | 7.2/18 | Pillar-tricot, 3.6 | — | — | B | AR glass | 1280/640 | 7.2/18 | Double tricot, 3.6 | — | — | C | AR glass | 640/1280 | 7.2/18 | Double tricot, 3.6 | — | — | D | AR glass | 1200/640 | 7.2/18 | Double tricot, 3.5 | Styrol butadiene | 30% | E | AR glass | 1200/1200 | 7.2/7.2 | Double tricot, 2.0 | Styrol butadiene | 30% | F | AR glass | 1200/640 | 7.2/10.2 | Double tricot, 2.0 | Styrol butadiene | 15% | G1 | Carbon | 800/800 | 10.8/18 | Double tricot, 3.5 | Styrol butadiene | 30% | G2a | Carbon | 800/800 | 10.8/18 | Double tricot, 3.5 | Epoxy resin | 30% | G2b | Carbon | 800/800 | 10.8/18 | Double tricot, 3.5 | Epoxy resin | 15% | H1a | Carbon4 | 800/640 | 7.2/18 | Double tricot, 3.5 | Styrol butadiene | 30% | H1b | Carbon4 | 800/640 | 7.2/18 | Double tricot, 3.5 | Styrol butadiene | 15% | H2 | Carbon4 | 800/640 | 7.2/18 | Double tricot, 3.5 | Epoxy resin | 15% |
|
|
1Between warp/weft yarns; 2of stitching fibre; 3of organic constituent in suspension; 4weft yarns made of AR glass.
|