Research Article
Compressive Strength and Microstructure Properties of Alkali-Activated Systems with Blast Furnace Slag, Desulfurization Slag, and Gypsum
| Mix. | OPC (O) | BFS (B) | DS (D) | Gypsum (G) |
| O100 | 100 | — | — | — | O50B50 | 50 | 50 | — | — | B95D5 | — | 95 | 5 | — | B90D10 | — | 90 | 10 | — | B85D15 | — | 85 | 15 | — | B80D20 | — | 80 | 20 | — | B75D25 | — | 75 | 25 | — | B70D30 | — | 70 | 30 | — | B81D10G9 | — | 81 | 10 | 9 | B78D10G12 | — | 78 | 10 | 12 | B75D10G15 | — | 75 | 10 | 15 |
|
|