Test mix of steel fiber concrete.
| Specimen number | Steel fiber parameter (%) | Steel fiber (kg) | Water (kg) | Cement (kg) | Coarse aggregate (kg) | Fine aggregate (kg) | Additive (kg) | Sand-coarse aggregate ratio |
| C50 | 0 | 0 | 172 | 347.5 | 1181.3 | 664.5 | 2.7 | 0.36 | 0.5 | 39 | 172 | 347.5 | 1159.5 | 674.3 | 2.7 | 0.36 | 1 | 58.9 | 172 | 347.5 | 1148.6 | 679.2 | 2.7 | 0.36 | 1.5 | 78.5 | 172 | 347.5 | 1137.8 | 684.9 | 2.7 | 0.36 | 2 | 117 | 172 | 347.5 | 1115.1 | 693.7 | 2.7 | 0.36 |
| C60 | 0 | 0 | 164 | 451.8 | 1078.2 | 660.8 | 4.9 | 0.36 | 0.5 | 39.3 | 164 | 451.8 | 1055.8 | 671.2 | 4.9 | 0.36 | 1 | 78.5 | 164 | 451.8 | 1033.5 | 681.5 | 4.9 | 0.36 | 1.5 | 117.8 | 164 | 451.8 | 1011.1 | 691.9 | 4.9 | 0.36 | 2 | 157 | 164 | 451.8 | 988.8 | 702.2 | 4.9 | 0.36 |
|
|