NoD (mm)H (mm) (kg/m3) (mm/s) (10−3) (MPa) Log(MPa/s)

2–148.73100.432423.870.0017.863.57−2.35
2–348.73101.022436.250.018.624.16−1.32
2–448.73100.482428.010.19.104.36−0.36
2–648.7399.932435.9919.754.660.67