286562.fig.004
Figure 4: Comparison of experimental and theoretical data. YIG [111] thickness is 110 μm; diameter is 2,5 mm; PMN-PT tickness is 0,5 mm; diameter is 6 mm. Field  Oe; field is parallel to plane of sample; average is 30; central frequency is 7251 MHz.