Formation of Porous Apatite Layer during In Vitro Study of Hydroxyapatite-AW Based Glass Composites
Figure 7
SEM micrographs on the surfaces of HA-AW composites sintered at 1100°C for 2 h, before and after soaking in the SBF solution at 37°C for 7 and 28 days.