Research Article

Formation of Porous Apatite Layer during In Vitro Study of Hydroxyapatite-AW Based Glass Composites

Table 2

Ion concentration of SBF solution in comparison with human blood plasma [18].

TypesIon concentrations (mM)
Na+K+Mg2+Ca2+Clāˆ’

SBF142.05.01.52.5148.84.21.0
Blood
plasma
142.05.01.52.5103.027.01.0