Research Article
Dispersion of Switching Processes in Ferroelectric Ceramics
Figure 1
Evolution of dielectric hysteresis loops of PZT ceramics exposed to AC sine field at the frequencies 220 (a), 600 (b), and 1500 Hz (c). V/mm, sample area 25 mm2.
(a) |
(b) |
(c) |