Research Article
Influence of Crystallization Time on Energy-Storage Density and Efficiency of Lead-Free Bi0.5(Na0.8K0.2)0.5TiO3 Thin Films
Figure 2
X-ray diffraction patterns of BNKT films in the 2θ ranges of (a) 28.0°–62.0°, (b) 30.0°–34.0°, and (c) 46.0°–48.5°.