Research Article
Performance of Sprayed Fiber Reinforced Polymer Strengthened Timber Beams
Table 3
Summary of results: creosoted.
| | Ultimate load (kN) | Ultimate displacement (mm) | Energy absorbed (kJ) | Load % increase over F | Energy absorbed % increase over F | FRP rupture |
| Beam F | 108.7 | 13.1 | 0.6 | — | — | — | Beam G | 139.3 | 35.6 | 3.6 | 28.2% | 460.1% | No | Beam H | 164.3 | 29.6 | 3.0 | 51.1% | 366.5% | No | Beam I | 112.4 | 29.9 | 2.5 | 3.4% | 287.4% | No | Beam J | 147.3 | 26.7 | 2.3 | 35.5% | 255.4% | Yes |
|
|