The Fabrication of Automobile Components by Applying Electromagnetic Stirring in Semisolid Process

Figure 21

Photographs of the knuckle part fabricated by various casting conditions.
232640.fig.0021a
(a) 0.25 m/s 450 bar
232640.fig.0021b
(b) 0.3 m/s 450 bar
232640.fig.0021c
(c) 0.5 m/s 450 bar