Figure 7

Photographs of arm part according to velocity and pressure (at 75% solid fraction): (1) 0.2 m/s and 300 bar; (2) 0.3 m/s and 300 bar; (3) 0.3 m/s and 450 bar; (4) 0.5 m/s and 450 bar.