Figure 6:
OM micrographs of T-joint (welding parameter:
KW,
υ
= 4 m/min). (a) Macrographs of the weld seam; (b) high magnification of spot A; (c) high magnification of spot B, (d) high magnification of spot C, and (e) High magnification of spot D.