Research Article

Stress Corrosion Cracking of Steel and Aluminum in Sodium Hydroxide: Field Failure and Laboratory Test

Figure 2

Appearance of C-ring specimen. Away from the areas of interest, coating was applied to avoid corrosion.
235028.fig.002a
(a)
235028.fig.002b
(b)
235028.fig.002c
(c)
235028.fig.002d
(d)
235028.fig.002e
(e)
235028.fig.002f
(f)