Research Article
Effects of Aging Temperature on Moisture Absorption of Perforated GFRP
Table 2
Bending test results for specimens aged at various temperatures (humidity 60%).
| Specimen/condition | Failure force (N)* | Maximum displacement (mm) | Stiffness, K (N/mm)* | Standard deviation |
| R-01/original | 176.05 | 2.2 | 82.5 | 0.104 | H 4/T = 40°C | 153.16 | 1.9 | 80.3 | 0.102 | H 6/T = 60°C | 139.08 | 1.8 | 78.2 | 0.104 | H 8/T = 80°C | 123.24 | 1.6 | 76.6 | 0.106 |
|
|
The reported data are the mean values of 3 results for each category.
|