Research Article

Structural and Phase Transformations in Water-Vapour-Plasma-Treated Hydrophilic TiO2 Films

Figure 4

XRD patterns of Ti film after plasma treatment: 1 as deposited, 2 for 5 min at 200 W, 3 for 20 min at 200 W, and 4 for 5 min at 300 W.
592485.fig.004