Research Article

The Influence of Na and Ti on the In Vitro Degradation and Bioactivity in 58S Sol-Gel Bioactive Glass

Figure 4

XRD patterns of the 58S, 58S6N, and 58S6T after immersion in SBF for 5 days.
730810.fig.004