Research Article

Aluminum Silicate Nanotube Modification of Cotton-Like Siloxane-poly(L-lactic acid)-vaterite Composites

Figure 2

(a) Calcium and (b) silicon amounts released from PLLA/SiV and PLLA/SiV-INT(10-5) after soaking in Tris buffer solution. Circle: PLLA/SiV, diamond: PLLA/SiV-INT(10-5).
169721.fig.002a
(a)
169721.fig.002b
(b)