232371.fig.007a
(a) SCCFA
232371.fig.007b
(b) SCCRHA
232371.fig.007c
(c) SCCOPC
232371.fig.007d
(d) SCCGGBS
Figure 7: Optical observation of the concrete exposed to MS, water and the drying age of SCC containing various SCM.