Research Article
Effect of Magnesium Sulphate on Self-Compacting Concrete Containing Supplementary Cementitious Materials
Table 7
Effect of MS on the mass with air drying SCC.
| Mix. no. | Mass (gr) | Magnesium sulphate | Air dried | Curing water | 44 d | 81 d | 118 d | 44 d | 81 d | 118 d | 44 d | 81 d | 118 d |
| SCCOPC | 2220 | 2240 | 2240 | 2222 | 2206 | 2202 | 2274 | 2340 | 2425 | SCCFA15 | 2460 | 2414 | 2402 | 2334 | 2332 | 2320 | 2480 | 2440 | 2480 | SCCRHA10 | 2365 | 2353 | 2342 | 2272 | 2265 | 2200 | 2375 | 2368 | 2386 | SCCGGBS5 | 2332 | 2320 | 2242 | 2246 | 2266 | 2280 | 2370 | 2382 | 2398 |
|
|