Research Article

Mechanical Characterization of Cryomilled Al Powder Consolidated by High-Frequency Induction Heat Sintering

Figure 10

True stress strain response in simple compression of consolidated samples at different sintering temperatures for a constant sintering time of 3 minutes in (a) and for different sintering times for a constant sintering temperature of 500°C. The heating rate used was 800°C/min.
397351.fig.0010a
(a)
397351.fig.0010b
(b)