Research Article

Mechanical Characterization of Cryomilled Al Powder Consolidated by High-Frequency Induction Heat Sintering

Figure 5

Effect of sintering temperature for the powders cryomilled for 7 hours for sintering of 3 minutes and high heating rate: (a) Vickers hardness, (b) percentage of full density, and (c) crystal size.
397351.fig.005a
(a)
397351.fig.005b
(b)
397351.fig.005c
(c)