Research Article

Misfit in Inconel-Type Superalloy

Figure 3

Examples of measured diffractograms of IN738LC. The fit by FullProf, decomposed also to its and parts, is plotted, too: (a) out-of-furnace (RT) measurement, (b) detail of 220 reflection for out-of-furnace measurement, (c) in-furnace (RT) measurement, and (d) in-furnace measurement at 800°C. The residuals (observed minus calculated intensity) are shown as well on the bottom part of Figures 3(a), 3(c), and 3(d).
408347.fig.003a
(a)
408347.fig.003b
(b)
408347.fig.003c
(c)
408347.fig.003d
(d)