Research Article
Behavior of HPC with Fly Ash after Elevated Temperature
Table 4
The cleavage strength of HPC at elevated temperature (MPa).
| Concrete | Temperature (°C) | 20 | 200 | 300 | 400 | 500 |
| C50 | 3.800 | 3.756 | 3.790 | 2.984 | 2.362 | C60 | 4.474 | 4.401 | 4.098 | 3.310 | 2.916 |
|
|