Research Article

Biopolymer Doped with Titanium Dioxide Superhydrophobic Photocatalysis as Self-Clean Coating for Lightweight Composite

Figure 7

Flexural strength of lightweight cube concrete with different ratio of WLA to cement (wt/wt): (A) 55%, (B) 60%, (C) 65%, and (D) 70%.
486253.fig.007