Research Article
Biopolymer Doped with Titanium Dioxide Superhydrophobic Photocatalysis as Self-Clean Coating for Lightweight Composite
Table 4
Flexural strength and density of standard and lightweight cube concrete with different ratio of WLA to cement (wt/wt).
| Types of composite | Composite percentages (wt/wt) | Samples | Load (N) | Flexural strength (MPa) | Deflection (mm) |
| Lightweight | WLA | 55% | A | 3330 | 1.499 | 1.16 | 60% | B | 3060 | 1.377 | 1.48 | 65% | C | 2690 | 1.211 | 0.98 | 70% | D | 490 | 0.221 | 0.08 |
| Standard composition | Commercial [8] | 3500 | 1.450 | 0.02 |
|
|