Research Article

High Temperature Deformation Behavior of 8090 Al-Li Alloy

Figure 3

Optical micrographs of thermomechanically treated 8090 Al-Li alloy with the average grain size of (a) 50 μm, (b) 18 μm, and (c) 10 μm, respectively.
512606.fig.003