Research Article

The Effect of Annealing on the Structural and Optical Properties of Titanium Dioxide Films Deposited by Electron Beam Assisted PVD

Figure 6

EDS spectrum of sample TAD measured from the interface layer. The strongest peaks belong to silicon and oxygen.
574738.fig.006