Preparation of CePO4 Modified ZrO2 Ceramics with Different Particle Sizes and Their Mechanical Behaviors

Figure 3

Linear shrinkage of the samples at different temperatures (1: 30–50 nm, uncoated; 2: 50–100 nm, uncoated; 3: 100–300 nm, uncoated; 4: 300–500 nm, uncoated; 5: 30–50 nm, coated; 6: 50–100 nm, coated; 7: 100–300 nm, coated; 8: 300–500 nm, coated).