Research Article
Optimization of Blending Parameters and Fiber Size of Kenaf-Bast-Fiber-Reinforced the Thermoplastic Polyurethane Composites by Taguchi Method
Table 6
Average of S/N ratio.
| Factor | Level 1 | Level 2 | Level 3
|
| Temperature A (°C) | 26.738 | 24.270 | 21.579 | Speed B (rpm) | 23.877 | 23.557 | 25.153 | Time C (min) | 24.192 | 24.817 | 23.578 | Size D (micron) | 22.933 | 24.956 | 24.698 |
|
|