Parameters Controlling the Oxide Reduction during Sintering of Chromium Prealloyed Steel

Figure 14

Microstructure and fracture surface of AstCrM + 0.8% C material sintered at 1200°C.
789373.fig.0014a
(a)
789373.fig.0014b
(b)