Parameters Controlling the Oxide Reduction during Sintering of Chromium Prealloyed Steel

Figure 6

Oxide inclusions in AstCrM + 0.5% C components’ densities of (a) 6.5, (b) 7.1, and (c) 7.4 g/cm3 sintered at 1200°C for 30 min.
789373.fig.006a
(a)
789373.fig.006b
(b)
789373.fig.006c
(c)