789373.fig.007a
(a)
789373.fig.007b
(b)
789373.fig.007c
(c)
Figure 7: Oxide inclusions in AstCrM + 0.5% C components’ densities of (a) 6.5, (b) 7.1, and (c) 7.4 g/cm3 sintered at 1120°C for 30 min.