Evaluation of Normal and Nanolayer Composite Thermal Barrier Coatings in Fused Vanadate-Sulfate Salts at 1000°C

Figure 9

Cross-section of the coatings after hot corrosion testing at 1000°C. (a, b) Conventional YSZ coating, (c) YSZ as inner layer of YSZ/normal Al2O3 coating, and (d) YSZ as inner layer of YSZ/nano-Al2O3 coating.