Research Article
Mechanical Properties of Recycled Aggregate Concrete at Low and High Water/Binder Ratios
Figure 5
Tensile splitting strength of concrete at W/B ratios of 0.255 and 0.586.
|
(a) For concrete at a W/B ratio of 0.255 |
|
|