Experimental Investigation on Material Transfer Mechanism in WEDM of Pure Titanium (Grade-2)

Figure 11

XRD pattern of the machined surface: (a) = 1.1 μs, = 28 μs, Ip = 200 A, SV = 50 V, WF = 7 m/min, WT = 500 grams; (b) = 0.7μs, = 28 μs, Ip = 120 A, SV = 50 V, WF = 7 m/min, WT = 500 grams.