Research Article

Experimental Investigation on Material Transfer Mechanism in WEDM of Pure Titanium (Grade-2)

Figure 5

SEM micrograph (1000x, 2000x, 3000x, and 500x): (a) experiment no. 1, at = 1.1 μs, = 28 μs, Ip = 200 A, SV = 50 V, WF = 7 m/min, WT = 500 grams; (b) experiment no. 35, at =1.1 μs, = 17 μs, Ip = 160 A, SV = 40 V, WF = 7 m/min, WT = 950 grams; (c) experiment no. 15, at = 0.7 μs, = 28 μs, Ip = 120 A, SV = 50 V, WF = 7 m/min, WT = 500 grams; (d) experiment no. 6, at = 1.1 μs, = 28 μs, Ip = 160 A, SV = 40 V, WF = 4 m/min, WT = 950 grams.
847876.fig.005a
(a)
847876.fig.005b
(b)
847876.fig.005c
(c)
847876.fig.005d
(d)