Research Article

Experimental Investigation on Material Transfer Mechanism in WEDM of Pure Titanium (Grade-2)

Figure 6

SEM micrograph (1000x, 2000x, 3000x, and 500x): (a) experiment no. 1, at = 1.1 μs, = 28 μs, Ip = 200 A, SV = 50 V, WF = 7 m/min, WT = 500 grams; (b) experiment no. 52, at = 1.1  μs, = 28  μs, Ip = 200 A, SV = 50 V, WF = 7 m/min, WT = 1400 grams; (c) experiment no. 50, at = 1.1  μs, = 17 μs, Ip = 160 A, SV = 60 V, WF = 7 m/min, WT = 950 grams; (d) experiment no. 36, at = 0.9  μs, = 17 μs, Ip = 200 A, SV = 50 V, WF = 10 m/min, WT = 950 grams.
847876.fig.006a
(a)
847876.fig.006b
(b)
847876.fig.006c
(c)
847876.fig.006d
(d)