927356.fig.003a
(a)
927356.fig.003b
(b)
Figure 3: FESEM micrograph of the as-spun Nd16Fe76B8/40% wt. Fe65Co35 ribbons: (a)  m/s without the assisted magnetic field and (b)  m/s in the magnetic field 0.32 T.