Effects of Electric Pulse Current on the Aging Kinetics of 2219 Aluminum Alloy
Figure 3
TEM images of 2219 aluminum alloy intracrystalline precipitations aged at 175°C. (a), (c) conventional aged for 12 h, 18 h; (b), (d) LEDPC added aged for 12 h, 18 h.