Research Article

Carbonation Characteristics of Alkali-Activated Blast-Furnace Slag Mortar

Figure 12

Differential thermograms (mass loss downwards) of noncarbonated (a) and carbonated (b) AAS mortar with different Na2O/S.M ratios.
326458.fig.0012a
(a)
326458.fig.0012b
(b)