Components of concrete (1 m3).
| Mix code | Waste tire (col%) | Waste tire (kg) | Portland cement (kg) | Sand (kg) | Gravel (kg) | Water (kg) |
| M0 | 0 | 0 | 337.1 | 758.5 | 662.6 | 286.3 | M10-7 | 10 | 36.2 | 337.1 | 596.4 | 758.5 | 278.4 | M20-7 | 20 | 72.4 | 337.1 | 530.1 | 758.5 | 270.6 | M30-7 | 30 | 108.7 | 337.1 | 463.8 | 758.5 | 262.7 | M10-20 | 10 | 47.2 | 337.1 | 596.4 | 758.5 | 278.4 | M20-20 | 20 | 94.5 | 337.1 | 530.1 | 758.5 | 270.6 | M30-20 | 30 | 141.7 | 337.1 | 463.8 | 758.5 | 262.7 |
|
|