Research Article

Mesostructural Design and Manufacturing of Open-Pore Metal Foams by Investment Casting

Figure 3

Evolution of strut thickening by PG1 at °C after thermal treatment of (a)  min, (b)  min, (c)  min, (d) min, (e) min, and (f)  min using the example of a polymer foam with a pore density of  ppi.
421729.fig.003a
(a)
421729.fig.003b
(b)
421729.fig.003c
(c)
421729.fig.003d
(d)
421729.fig.003e
(e)
421729.fig.003f
(f)