Research Article

Effects of Rolling Reduction and Strength of Composed Layers on Bond Strength of Pure Copper and Aluminium Alloy Clad Sheets Fabricated by Cold Roll Bonding

Figure 8

Fractured interface after tensile shear tests, (a) Cu/Al-50%, (b) Cu/Al-75%, (c) Cu/AA5052-50%, (d) Cu/AA5052-75%, (e) Cu/AA5083-50%, and (f) Cu/AA5083-75%.
614821.fig.008