Functionalization of Natural Cork Composite with Microcapsules after Plasma Treatment

Figure 3

FTIR-ATR (a) and atomic percentage by EDS (b) of the cork agglomerate samples untreated and plasma treated (2400 W·min·m−2).
685829.fig.003a